Diameter (mm) | Length (mm) | surface condition | |||||||||
1-100 | 50-2000 | Alkali washing, pickling, polishing |
number | Chemical composition (mass fraction, %) | |||||||||||||
Main ingredient | Impurity ≤ | |||||||||||||
Mo | Ti | Zr | C | Al | Ca | Fe | Mg | Ni | Si | C | N | O | ||
TZM | margin | 0.4-0.55 | 0.06-0.121 | 0.01-0.04 | - | - | 0.01 | - | 0.005 | 0.01 | - | 0.003 | 0.08 |
material | Density g/cm 3 | Melting point °C | Boiling point °C |
TZM alloy (Ti0.5/Zr0.1) | 10.22 | 2617 | 4612 |
Mo | 10.29 | 2610 | 5560 |
Mechanical properties | Elongation | Elastic Modulus | Yield Strength | tensile strength | Fracture toughness |
Numerical value | <20 | 320 | 560-1150 | 685 | 5.8-29.6 |
Temperature / °C | performance | |
Tensile strength / MPa | Elongation % | |
RT | 1140 ~ 1210 | 7.5~13.0 |
1000 | 1000 | 700 ~ 720 |
1200 | 1200 | 320 ~ 360 |
1300 | 1300 | 190 ~ 210 |
1400 | 1400 | 140 ~ 170 |
performance | Thermal expansion coefficient / K-1 (20 ~ 100 ° C) | Thermal conductivity W/m·K | Maximum operating temperature in air °C | Resistivity Ω·m |
Numerical value | 5.3*10 -6 | 126 | 400 | (5.3-5.5)*10 -8 |